Material Notes:
Application: 105°C rated jacketing compound with good low temperature and aging properties.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87.0

@Time 15.0 sec
87.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 17.2 MPa
2490 psi
ASTM D412
17.2 MPa

@Temperature 136 °C,
Time 605000 sec
2490 psi

@Temperature 277 °F,
Time 168 hour
Oven Aged
Elongation at Break 300 %
300 %
ASTM D412
225 %

@Treatment Temp. 136 °C,
Time 605000 sec
225 %

@Treatment Temp. 277 °F,
Time 168 hour
Oven Aged
Thermal Properties Metric English Comments
Brittleness Temperature -24.0 °C
-11.2 °F
ASTM D746
Oxygen Index 30.0 %
30.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 171 - 177 °C
340 - 350 °F
Suggested Stock