Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufTech™ GA-8705-03 Natural Gloss PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GA-8705-03 Natural Gloss PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: 75°C lead free, RoHS compliant riser jacketing compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82.0

@Time 15.0 sec
82.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Elongation at Break 275 %
275 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -18.0 °C
-0.400 °F
ASTM D746
Oxygen Index 29.5 %
29.5 %
ASTM D2863