S&E Specialty Polymers TufTech™ GA-93-016AGH PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GA-93-016AGH PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A RoHS Compliant, Flame Retardant 60/75?C Jacketing Compound.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84.0

@Time 15.0 sec
84.0

@Time 0.00417 hour
Fresh; ASTM D2240
90.0

@Time 15.0 sec
90.0

@Time 0.00417 hour
24 hr values; ASTM D2240
Tensile Strength 17.9 MPa
2600 psi
ASTM D412
Elongation at Break 275 %
275 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature <= -18.0 °C
<= -0.400 °F
ASTM D746
Oxygen Index 29.0 %
29.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 177 - 182 °C
350 - 360 °F
Suggested Extrusion