S&E Specialty Polymers TufTech™ GM-3236 PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer S&E Specialty Polymers
Trade Name TufTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufTech™ GM-3236 PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: A non-toxic PVC based compound designed for general purpose profile extrusion applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65.0

@Time 15.0 sec
65.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 13.4 MPa
1940 psi
ASTM D412
Elongation at Break 360 %
360 %
ASTM D412