Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Graphite filler with isotrope structureInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Bulk Density 0.450 g/cc
0.0163 lb/in³
0.760 g/cc
0.0275 lb/in³
Tap Density
Density 2.22 g/cc
0.0802 lb/in³
Real Density
Particle Size <= 1.0 µm
<= 1.0 µm
2%
<= 8.0 µm
<= 8.0 µm
31%
<= 32 µm
<= 32 µm
78%
<= 64 µm
<= 64 µm
96%
<= 96 µm
<= 96 µm
100%
Specific Surface Area 0.833 m²/g
0.833 m²/g
Blaine
Ash <= 1.0 %
<= 1.0 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %