SGL Carbon Group EK 200 Graphite

Category Carbon , Graphite
Manufacturer SGL Carbon Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SGL Carbon Group EK 200 Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Bearings, seals for compressorsCertified for use in potable water and/or in foodstuff; Certified for use in oxygenous atmosphereInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
Open Porosity <= 2.5 %
<= 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
Size/Load - 10/150
Hardness, Shore C 107
107
Modulus of Elasticity 13.8 GPa
2000 ksi
Flexural Strength 48.3 MPa
7000 psi
Compressive Strength 221 MPa
32000 psi
Thermal Properties Metric English Comments
CTE, linear 7.74 µm/m-°C

@Temperature 20.0 °C
4.30 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 25.9 W/m-K
180 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
In oxygen
Maximum Service Temperature, Inert 204 °C
399 °F
Reducing Atm.
Descriptive Properties Value Comments
Impregnation Resin