Material Notes:
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and good electrical conductivity.Typical Applications: Dry Running SealsInformation provided by SGL Carbon Group
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Open Porosity <= 2.5 %
<= 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
Size/Load - 5/100
Hardness, Shore C 105
105
Modulus of Elasticity 24.1 GPa
3500 ksi
Flexural Strength 79.3 MPa
11500 psi
Compressive Strength 248 MPa
36000 psi
Thermal Properties Metric English Comments
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 20.8 W/m-K
144 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 399 °C
750 °F
In oxygen
Maximum Service Temperature, Inert 538 °C
1000 °F
Reducing Atm.
Descriptive Properties Value Comments
Impregnation Antimony