Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 3840 EA MDPE Wire and Cable Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 3840 EA MDPE Wire and Cable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Suitable for the production of silane cross-linkable compoundsLow voltage power cable insulationInjection molded technical parts and closureInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ISO 1872/1
Environmental Stress Crack Resistance 200 hour

@Temperature 30.0 °C
200 hour

@Temperature 86.0 °F
F50; ASTM D1693
Melt Flow 4.0 g/10 min

@Load 2.16 kg
4.0 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
BP 13B/1
Elongation at Break 1210 %
1210 %
BP 13B/1
Flexural Modulus 0.750 GPa
109 ksi
ISO 178-1975
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179