Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 3840 UA MDPE Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 3840 UA MDPE Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Rotational items: tanks, containers, etc...Injection molded technical parts and closureInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ISO 1872/1
Environmental Stress Crack Resistance 200 hour
200 hour
F50; BP 13C/25
Melt Flow 4.0 g/10 min

@Load 2.16 kg
4.0 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
BP 13B/1
Elongation at Break 1400 %
1400 %
BP 13B/1
Flexural Modulus 0.650 GPa
94.3 ksi
ISO 178-1975
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179