Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 5301 FB HDPE Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 5301 FB HDPE Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ISO 1872/1
Thickness 15.0 microns
0.591 mil
Melt Flow 0.050 g/10 min

@Load 2.16 kg
0.050 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 32.0 MPa
4640 psi
ISO 1184
Film Tensile Strength at Yield, TD 29.0 MPa
4210 psi
ISO 1184
Film Elongation at Break, MD 450 %
450 %
ISO 1184
Film Elongation at Break, TD 400 %
400 %
ISO 1184
Dart Drop 10.0 g/micron
254 g/mil
Calculated from thickness
Dart Drop Test 150 g
0.331 lb
ASTM D1709
Film Tensile Strength at Break, MD 56.0 MPa
8120 psi
ISO 1184
Film Tensile Strength at Break, TD 65.0 MPa
9430 psi
ISO 1184
Users viewing this material also viewed the following: