Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® LL 0205 AF LLDPE Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® LL 0205 AF LLDPE Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1872/1
Thickness 38.0 microns
1.50 mil
Melt Flow 0.50 g/10 min

@Load 2.16 kg
0.50 g/10 min

@Load 4.76 lb
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.0 MPa
1450 psi
ISO 1184
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 1184
Film Elongation at Break, MD 600 %
600 %
ISO 1184
Film Elongation at Break, TD 790 %
790 %
ISO 1184
Elmendorf Tear Strength, MD 6.10 g/micron
155 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 14.8 g/micron
375 g/mil
ASTM D1922
Dart Drop 4.74 g/micron
120 g/mil
Calculated from thickness
Dart Drop Test 180 g
0.397 lb
ASTM D1709
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
ISO 1184
Film Tensile Strength at Break, TD 35.0 MPa
5080 psi
ISO 1184
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 225 °C
437 °F
Copyright © lookpolymers.com All Rights Reserved