Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SK Chemicals SKYTHANE® 875A T series Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® 875A T series Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
ASTM D2240
Hardness, Shore D 32
32
ASTM D2240
Tensile Strength, Ultimate 31.4 MPa
4550 psi
ASTM D412
Tensile Strength, Yield 3.53 MPa

@Strain 100 %
512 psi

@Strain 100 %
ASTM D412
7.35 MPa

@Strain 300 %
1070 psi

@Strain 300 %
ASTM D412
Elongation at Break 700 %
700 %
ASTM D412
Resilience 50
50
by vertical rebound; ASTM D2632
Tear Strength 93.2 kN/m
532 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 15
15
H18 Wheel; 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 81.0 °C
178 °F
ASTM D1525