SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets and FilmHoses and TubingShoe ComponentsFire HosesInformation provided by SK Chemicals.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Hardness, Shore D 53
53
ASTM D2240
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
100% Modulus 0.0159 GPa
2.30 ksi
ASTM D412
300% Modulus 0.0352 GPa
5.10 ksi
ASTM D412
Resilience 37
37
Vertical Rebound; ASTM D2632
Tear Strength 137 kN/m
784 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
30
H18 wheel, 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 205 °C
401 °F
Transition Temperature
205 °C
401 °F
Metering Temperature
Middle Barrel Temperature 200 °C
392 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 190 °C
374 °F
Zone 2 195 °C
383 °F
Zone 3 200 °C
392 °F
Zone 4 205 °C
401 °F
Adapter Temperature 205 °C
401 °F
Die Temperature 205 °C
401 °F
Tip
210 °C
410 °F
Body
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F