SPS Guang Zhou SAMATâ„¢ 5003 Flame-retarded Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer SPS Guang Zhou
Trade Name SAMAT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou SAMATâ„¢ 5003 Flame-retarded Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: Good chemical resistance, good mechanical properties, excellent long-term thermal stabilityApplications: E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Flexural Strength 42.0 MPa
6090 psi
Flexural Modulus 1.50 GPa
218 ksi
Izod Impact, Notched 0.700 J/cm
1.31 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Flammability, UL94 V-2
V-2