Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SSAB Tunnplat Docol® 800 DP High-strength Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Docol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Docol® 800 DP High-strength Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 800 - 900 MPa
116000 - 131000 psi
Tensile Strength, Yield >= 650 MPa
>= 94300 psi
After bake hardening
500 - 650 MPa

@Strain 0.200 %
72500 - 94300 psi

@Strain 0.200 %
Elongation at Break >= 8.0 %
>= 8.0 %
A<sub>80</sub>
Bend Radius, Minimum >= 1.0 t
>= 1.0 t
t = 1.0 mm
>= 2.0 t
>= 2.0 t
t = 1.5 mm
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 %
0.040 %
Carbon, C 0.12 %
0.12 %
Iron, Fe 98 %
98 %
As remainder
Manganese, Mn 1.5 %
1.5 %
Niobium, Nb (Columbium, Cb) 0.015 %
0.015 %
Phosphorous, P 0.015 %
0.015 %
Silicon, Si 0.20 %
0.20 %
Sulfur, S 0.0020 %
0.0020 %
Users viewing this material also viewed the following: