SSAB Tunnplat Domex® 700MC HSLA Steel

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer SSAB Tunnplat AB
Trade Name Domex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SSAB Tunnplat Domex® 700MC HSLA Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of benefits compared to ordinary structural steels: Lower weight, Simpler production, Lower creep rate, Longer useful life, Higher load-bearing capacity, Lower transport costs, Reduced stocks, Lower overall cost.Data provided by SSAB Tunnplat.
Physical Properties Metric English Comments
Density 7.87 g/cc
0.284 lb/in³
Estimated by MatWeb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 750 - 950 MPa
109000 - 138000 psi
Tensile Strength, Yield >= 700 MPa
>= 102000 psi
Elongation at Break >= 10 %

@Thickness <=3.00 mm
>= 10 %

@Thickness <=0.118 in
A<sub>80</sub>
>= 12 %

@Thickness >=3.00 mm
>= 12 %

@Thickness >=0.118 in
A<sub>5</sub>
Impact 71
71
J/cm²; -20°C
52.0

@Temperature -40.0 °C
52.0

@Temperature -40.0 °F
J/cm²
Bend Radius, Minimum >= 1.0 t
>= 1.0 t
t<3mm; internal bend radius, 90°
>= 1.5 t
>= 1.5 t
3 mm < t< 6mm; internal bend radius, 90°
>= 2.0 t
>= 2.0 t
t>6mm; internal bend radius, 90°
Component Elements Properties Metric English Comments
Aluminum, Al >= 0.015 %
>= 0.015 %
Boron, B <= 0.0050 %
<= 0.0050 %
Carbon, C <= 0.12 %
<= 0.12 %
Iron, Fe 97 %
97 %
As remainder
Manganese, Mn <= 2.1 %
<= 2.1 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.30 %
<= 0.30 %
Sulfur, S <= 0.010 %
<= 0.010 %
Users viewing this material also viewed the following: