Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

STAR Thermoplastic Alloys & Rubbers StarMediflex P 7095-1000 TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer STAR Thermoplastic Alloys & Rubbers
Trade Name StarMediflex
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF STAR Thermoplastic Alloys & Rubbers StarMediflex P 7095-1000 TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: StarMediflex P 7095-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:Soft TouchRubbery FeelExcellent ColorabilityProcessing Method: Injection MoldingInformation Provided by STAR Thermoplastic Elastomers
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95

@Time 10.0 sec
95

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 5.01 MPa

@Time 7200 sec
726 psi

@Time 2.00 hour
Die C; ASTM D414
Elongation at Break 726 %

@Time 7200 sec
726 %

@Time 2.00 hour
Die C; ASTM D412
300% Modulus 0.00345 GPa

@Time 7200 sec
0.500 ksi

@Time 2.00 hour
Die C; ASTM D412
Tear Strength 32.6 kN/m
186 pli
ASTM D624
Descriptive Properties Value Comments
Color Translucent
Users viewing this material also viewed the following: