Material Notes:
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into thick walled products and blocks. Lower density can be achieved after several preforming operations.Specific Characteristics: Flammability according to CSN EN ISO 11925-2, class E and DIN 4102-B1.Typical Application: Large volume products. Plates and cut profiles. Boards for external insulation of walls of buildings acc CSN EN 13163.Synthos was formerly known as Kaucuk. All information provided by Synthos.
Physical Properties Metric English Comments
Bulk Density >= 0.0120 g/cc
>= 0.000434 lb/in³
Typical
0.0230 g/cc
0.000831 lb/in³
Minimum
Particle Size 1250 - 1600 µm
1250 - 1600 µm