Saint-Gobain CHR® A602 Aluminum Foil Backing Silicone Adhesive Pressure Sensitive Tape

Category Polymer , Adhesive , Tape , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name CHR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain CHR® A602 Aluminum Foil Backing Silicone Adhesive Pressure Sensitive Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requiring higher tear strengths. Service temperatures range from -100°F to +500°F (-73°C to +260°C). Applications include thermal spray, aircraft repainting, EMI/RFI shielding, and electroplating. This tape uses a silicone adhesive system. Perfect for extreme temperature applications, silicone adhesives perform in continuous operating temperatures from -100°F to 500° (-73°C to 260°C). Silicone-based adhesive systems exhibit good chemical resistance, retain electrical properties, and remove cleanly with little or no residue. All data based on a 0.004 inch test sample.(Thickness given is for both backing and adhesive. Backing thickness is .002 inches.) Information provided by Saint Gobain Performance Products.
Mechanical Properties Metric English Comments
Elongation at Break <= 8.0 %
<= 8.0 %
Tear Strength 3.51 kN/m
20.0 pli
Initial Tear Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Descriptive Properties Value Comments
Color Aluminum