Material Notes:
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series can be machined into various confiations, from rod or sheet stock shapes. Black in color. Meldin 2000 Series offers very high compression strength, high creep resistance, and dimensional stability.Specific Notes on Meldin 2211 BearingMeldin 2211 offers the balanced properties of low friction, high strength and resistance to compressive creep.Applications include: Appliances, Automotive, Industrial, Semiconductor, Transportation.Specification Notes: Note that the specifications given for this product are typical specifications for the Meldin 2000 Series, and individual products will vary as indicated in the material notes.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Water Absorption 0.18 %
0.18 %
ASTM D570
Deformation 0.10 %

@Pressure 13.8 MPa
0.10 %

@Pressure 2000 psi
24 hrs. Mold Direction; ASTM D621
Outgassing - Total Mass Loss 0.010 %
0.010 %
% CVCM; ASTM E55955
0.50 %
0.50 %
% WVR; ASTM E595
1.19 %
1.19 %
% TML; ASTM E5955
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength, Ultimate 22.0 MPa

@Temperature 260 °C
3190 psi

@Temperature 500 °F
ASTM D 638
46.8 MPa

@Temperature 23.0 °C
6790 psi

@Temperature 73.4 °F
ASTM D 638
Elongation at Break 3.0 %

@Temperature 260 °C
3.0 %

@Temperature 500 °F
ASTM D 638
4.0 %

@Temperature 23.0 °C
4.0 %

@Temperature 73.4 °F
ASTM D 638
Tensile Modulus 0.700 GPa

@Temperature 260 °C
102 ksi

@Temperature 500 °F
ASTM D 638
2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
ASTM D 638
Flexural Strength 79.2 MPa
11500 psi
ASTM D 790
Flexural Modulus 3.80 GPa
551 ksi
ASTM D 790
Izod Impact, Notched 0.198 J/cm
0.371 ft-lb/in
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C
32.2 µin/in-°F
ASTM E831-93
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
C518/C177
Maximum Service Temperature, Air >= 316 °C
>= 600 °F
UL-746 B
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Constant 5.47

@Frequency 1.00e+6 Hz
5.47

@Frequency 1.00e+6 Hz
ASTM D150
5.53

@Frequency 10000 Hz
5.53

@Frequency 10000 Hz
ASTM D150
5.56

@Frequency 100 Hz
5.56

@Frequency 100 Hz
ASTM D150
Dissipation Factor 0.0019

@Frequency 100 Hz
0.0019

@Frequency 100 Hz
ASTM D150
0.0028

@Frequency 10000 Hz
0.0028

@Frequency 10000 Hz
ASTM D150
0.0035

@Frequency 1.00e+6 Hz
0.0035

@Frequency 1.00e+6 Hz
ASTM D150