Material Notes:
Meldin 3130 components provide good strength and stiffness in addition to excellent high velocity performance. This formulation can be used with both hard or soft mating surfaces. Meldin® 3100 materials have excellent mechanical properties, in tension and compression, and maintain an impressive level of these attributes as operating temperatures increase. These properties add extreme strength and rigidity to component parts, even in narrow cross-sections.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 133.59 MPa
19376 psi
ASTM D638
Elongation at Yield 5.2 %
5.2 %
ASTM D638
Tensile Modulus 3.83 GPa
556 ksi
ASTM D 638
Flexural Strength 222.5 MPa
32270 psi
ASTM D790
Flexural Modulus 18.52 GPa
2686 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C
421 °F
ASTM D648
Glass Transition Temp, Tg 233 °C
451 °F