Saint-Gobain Meldin® 7001 Direct Formed Polyimide

Category Polymer , Thermoset , Polyimide, TS
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 7001 Direct Formed Polyimide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high temperature resistance. Applications include: plasma cutting torch components, plasma etch equipment clamp rings, aerospace components, semiconductor equipment components.Specification Qualifications: ASTM D 6456-99 Standard Specification for Finished Parts Made from Polyimide Resin (Type I D). SAE AMS 3644G Polyimide, Molded Rod, Bar and Tube, Plaque, and Formed Parts (Class 1 Form D). MIL-R-46198 Resin, Polyimide, Hot Pressed or Pressed and Sintered (Type I D).
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Deformation 0.10 %
0.10 %
2000 psi load; ASTM D621
0.00 %

@Temperature 260 °C
0.00 %

@Temperature 500 °F
High Temp Dimensional Stability
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 75.8 MPa
11000 psi
ASTM D638
36.5 MPa

@Temperature 300 °C
5290 psi

@Temperature 572 °F
ASTM D638
41.3 MPa

@Temperature 260 °C
5990 psi

@Temperature 500 °F
ASTM D638
62.0 MPa

@Temperature 110 °C
8990 psi

@Temperature 230 °F
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
7.5 %

@Temperature 260 °C
7.5 %

@Temperature 500 °F
ASTM D638
Flexural Strength 88.3 MPa
12800 psi
ASTM D790
48.0 MPa

@Temperature 260 °C
6960 psi

@Temperature 500 °F
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
1.40 GPa

@Temperature 260 °C
203 ksi

@Temperature 500 °F
ASTM D790
Compressive Strength 22.1 MPa
3200 psi
1% strain; ASTM D695
96.5 MPa
14000 psi
10% strain; ASTM D695
Compressive Modulus 2.00 GPa
290 ksi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 4.86 µm/m-°C

@Temperature 22.8 - 260 °C
2.70 µin/in-°F

@Temperature 73.0 - 500 °F
ASTM E831
Thermal Conductivity 0.317 W/m-K
2.20 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 316 °C
600 °F
Minimum Service Temperature, Air -80.0 °C
-112 °F
Flammability, UL94 V-0
V-0
5VA
5VA
Electrical Properties Metric English Comments
Dielectric Strength 23.5 kV/mm
597 kV/in
ASTM D149
Descriptive Properties Value Comments
Color Brown