Saint-Gobain Norton® ECTFE Fluoropolymer Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , ETFE/ECTFE
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® ECTFE Fluoropolymer Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon-flammableThermoformableProduct thicknesses from 0.0005" (0.013 mm) to 0.010" (0.254 mm)Width up to 60" (1524 mm)Blue, clear, and white colorsAll films are manufactured and converted in class 100,000 clean room facilityNorton® ECTFE fluoropolymer film is manufactured from ethylene-chlorotrifluoroethylene (Halar®, a registered trademark of Ausimont USA, Inc) resin by Saint-Gobain Advanced Films and Fabrics. This material offers the outstanding performance of fluoropolymer film over a temperature range from cryogenic -200°C (-328°F) to 165°C (330°F).Norton® ECTFE film provides the highest abrasion resistance of any fluoropolymer film available. This film has superior chemical resistance and very high tensile strength and flexural modulus.Norton® ECTFE film offers low surface energy, making it an excellent choice for release applications. The low specific gravity of ECTFE provides more square feet than FEP for composite fabrication.The combination of heat stability, electrical characteristics, and barrier properties provides insulator performance especially suited for the electrical and electronics industry. Norton® ECTFE film offers the highest dielectric strength of all fluoropolymer films.Norton® ECTFE film has outstanding resistance to weathering and high energy radiation. This material is suited for electrical tapes, cable insulation, printed circuits, capacitors, chlorine cells, flat cable constructions, and solar collectors.Norton® ECTFE film offers a UL V-0 rating for flammability. This provides performance suitable for aircraft cabin interiors and fuel cell membranes.Used primarily for Aerospace/Release films, Chemical Process, Electrical/ElectronicsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D-792
Water Absorption <= 0.010 %
<= 0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D-882
Elongation at Break 250 %
250 %
ASTM D-882
Tensile Modulus 1.38 GPa
200 ksi
ASTM D-882
Tear Strength 177 kN/m
1010 pli
Initial Tear Strength; ASTM D-1004
Elmendorf Tear Strength, MD >= 47.2 g/micron
>= 1200 g/mil
(direction not reported), Propagation Tear Strength; ASTM D-1922
Heat Seal Strength Initiation Temperature 246 - 260 °C
475 - 500 °F
Thermal Properties Metric English Comments
CTE, linear 162 µm/m-°C

@Temperature 20.0 °C
90.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Melting Point 241 °C
465 °F
ASTM D-3418
Maximum Service Temperature, Air 149 - 171 °C
300 - 340 °F
UL-746 B
Flammability, UL94 V-0
V-0
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
ASTM D542
Electrical Properties Metric English Comments
Dielectric Constant 2.55 - 2.63

@Frequency 1000 Hz
2.55 - 2.63

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 217 kV/mm
5500 kV/in
ASTM D-149
Dissipation Factor <= 0.0050
<= 0.0050
ASTM D-150
Descriptive Properties Value Comments
Fold Endurance (MIN) 250000
ASTM D2176