Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.001" thick)

Category Polymer , Film , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton® Fluorglas® Chemfilm®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.001" thick).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet the requirements for MIL-P-22241B, type II, grade A and MIL-W-22759. R19 Virgin Description: Skived tapes and S-100 Virgin Description: Skived film have enhanced sealing capabilities. PTFE = polytetrafluoroethyleneInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
Longitudinal
Elongation at Break 275 %
275 %
ASTM D-882
Electrical Properties Metric English Comments
Dielectric Strength 157 kV/mm
4000 kV/in
ASTM D-149
Users viewing this material also viewed the following: