Saint-Gobain Norton® High Performance Extruded PEI Film

Category Polymer , Film , Thermoplastic , Polyetherimide (PEI)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® High Performance Extruded PEI Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D-792
Water Absorption 0.50 %
0.50 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 107 MPa
15500 psi
ASTM D-882
Elongation at Break 105 %
105 %
ASTM D-882
Tensile Modulus 2.59 GPa
375 ksi
ASTM D-882
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature 20.0 °C
30.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Maximum Service Temperature, Air 227 °C
440 °F
UL-746 B
Flammability, UL94 V-0
V-0
VTM-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.80e+16 ohm
1.80e+16 ohm
ASTM D-257
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 244 kV/mm
6200 kV/in
ASTM D-149
Dissipation Factor 0.0020
0.0020
ASTM D-150