Saint-Gobain Norton® PVDF Fluoropolymer Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® PVDF Fluoropolymer Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from 0.001" (0.0254 mm) to 0.020" (0.5 mm)Temperature range of -62°C (-80°F) to 150°C (300°F)Weatherable, Chemically Resistant Fluoropolymer FilmNorton® PVDF film is manufactured from polyvinylidene fluoride resin. This product offers the best weathering characteristics of any fluoropolymer film available. Norton® PVDF provides very good performance when subjected to severe conditions such as heat fluctuation, UV exposure, and corrosive environments. Norton® PVDF is manufactured to strict standards for gels and gauge control, offering the best value for fluoropolymer performance of any film. This material also performas over a wide temperature range, from -62°C (-80°F) to 150°C (300°F).Chemical ProtectionNorton® PVDF film protects against exposure to many common acids, oxidizing agents, and organics. This broad range of chemical resistance makes Norton® PVDF an excellent candidate for pump diaphragms and tank linings. The thin gauge films offer bondability for protection of equipment exposed to air pollutants, corrosive media, and weather.Decorative ApplicationsNorton® PVDF film can be adaptable to metallizing or printing for a variety of protective applications. The excellent chemical resistance to a wide tange of cleaners and harsh cleaning agents used in high traffic applications offers long maintenance performance. Norton® PVDF carries a UL V-0 flammability rating, which signifies self-extinguishing performance suited for aircraft interior panel applications.Weathering ApplicationsThe outstanding weatherability of Norton® PVDF film makes it an excellent candidate for products with outdoor exposures. Vinyl siding is protected with excellent chemical and abrasion resistance of Norton® PVDF film. The fluoropolymer properties are impervious to UV expsure and eliminate wear due to water and chemical exposures. PVDF = polyvinylidene fluorideUsed for Chemical Process, Electrical/Electronics, Protective/Decorative.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D-792
Water Absorption <= 0.040 %
<= 0.040 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 - 49.6 MPa
5000 - 7200 psi
ASTM D-882
Elongation at Break 100 - 250 %
100 - 250 %
ASTM D-882
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-882
Thermal Properties Metric English Comments
CTE, linear 119 - 139 µm/m-°C

@Temperature 20.0 °C
66.0 - 77.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Specific Heat Capacity 1.17 - 1.59 J/g-°C
0.280 - 0.380 BTU/lb-°F
Thermal Conductivity 0.199 W/m-K
1.38 BTU-in/hr-ft²-°F
ASTM D-2863
Melting Point 174 °C
345 °F
ASTM D-3418
Maximum Service Temperature, Air 129 °C
265 °F
UL-746 B
Flammability, UL94 V-0
V-0
Oxygen Index >= 44 %
>= 44 %
ASTM D2863
Optical Properties Metric English Comments
Refractive Index 1.40
1.40
ASTM D542
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+14 ohm
1.00e+14 ohm
ASTM D-257
Dielectric Constant 8.2 - 10

@Frequency 1000 Hz
8.2 - 10

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 157 kV/mm
4000 kV/in
ASTM D-149
Dissipation Factor 0.0050 - 0.020
0.0050 - 0.020
ASTM D-150
Descriptive Properties Value Comments
Fold Endurance (MIN) 26000
ASTM D2176