Category Ceramic , Glass , Glass Fiber , Oxide , Silicon Oxide , Other Engineering Material , Composite Fibers
Manufacturer Saint-Gobain Quartz PLC
Trade Name Quartzel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Quartzel® Fused Quartz Textiles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is available in the form of yarn, roving, chopped strands, wool, and felts.It is used in dielectric applications (radomes, circuit boards), thermal applications (high temp insulation for aerospace, asbestos replacement, furnace linings, hot gas filtration), and reinforcement for composites (with resins such as phenolics or epoxies). Information provided by Saint-Gobain Quartz PLC.
Physical Properties Metric English Comments
Density 2.20 g/cc
0.0795 lb/in³
Mechanical Properties Metric English Comments
Hardness, Mohs 7.0
7.0
Tensile Strength, Ultimate 6000 MPa
870000 psi
Virgin Filament
Elongation at Break 7.7 %
7.7 %
Virgin Filament
Modulus of Elasticity 78.0 GPa
11300 ksi
Virgin Filament
Poissons Ratio 0.16
0.16
Thermal Properties Metric English Comments
CTE, linear 0.540 µm/m-°C

@Temperature 20.0 °C
0.300 µin/in-°F

@Temperature 68.0 °F
isotropic (axial vs. radial)
Specific Heat Capacity 0.750 J/g-°C
0.179 BTU/lb-°F
Thermal Conductivity 1.38 W/m-K
9.58 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1050 °C
1920 °F
Softening Point 1700 °C
3090 °F
Annealing Point 1220 °C
2230 °F
Optical Properties Metric English Comments
Refractive Index 1.4585
1.4585
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+10 ohm-cm

@Temperature 800 °C
6.00e+10 ohm-cm

@Temperature 1470 °F
Dielectric Constant 3.74

@Frequency 1e+9 Hz
3.74

@Frequency 1e+9 Hz
Dielectric Strength 37.0 kV/mm
940 kV/in
Dissipation Factor 0.00020

@Frequency 1e+9 Hz
0.00020

@Frequency 1e+9 Hz