Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygothane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygothane® C-210-A Precision Polyurethane Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Tygothane® C-210-A: Our rigidly controlled manufacturing process makes Tygothane® Precision Polyurethane Tubing the flexible polyurethane tubing that has consistently tight tolerances from lot to lot. Precision tolerances and high elasticity provide the user with an easy, worry-free attachment to fittings. Made of a tough, ester-based polyurethane, Tygothane® Precision Polyurethane Tubing's clarity, high tear strength and excellent abrasion resistance make it ideal for many applications, including fuel and lubricant lines, pneumatic lines, abrasive product transfer and cable jacketing. It also offers exceptional resistance to oils, greases, fuels and many chemicals. Able to withstand rugged daily use, Tygothane® Precision Polyurethane Tubing resists weathering and can be safely used in temperatures ranging from -100°F (-73°C) to 200°F (93°C). It meets FDA criteria for food and beverage use and is also available in ether-based, medical grade and reinforced formulations.Features/Benefits:Consistently tight dimensional tolerancesExcellent abrasion and tear resistanceExcellent resistance to oils, greases and fuelsHigh tear resistanceRetains flexibility in sub-zero environmentsMeets FDA criteriaTypical applications include Food and Cosmetic Processing, Abrasive and Viscous Slurry Transfer, Lubrication and Degreaser Dispensing, pellet and Powder Transfer, Pneumatic Sensory Devices, Instrumentation Control Lines, Coolant Recovery SystemsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792-98
Water Absorption 1.12 %
1.12 %
24 hours at 23°C; ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
15 seconds; ASTM D2240-97
Tensile Strength, Yield 41.7 MPa
6050 psi
ASTM D412-98
Elongation at Break 500 %
500 %
ASTM D412-98
100% Modulus 0.00552 GPa
0.800 ksi
ASTM D412-98
300% Modulus 0.0103 GPa
1.50 ksi
ASTM D412-98
Tear Strength 83.3 kN/m
475 pli
Initial Tear Strength; ASTM D1004-94
Compression Set 68 %

@Temperature 70.0 °C
68 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-98 Method B
Tensile Set 98 %
98 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.4 °C
175 °F
93.3 °C
200 °F
Intermittent
Brittleness Temperature -73.3 °C
-100 °F
ASTM D746-98
Electrical Properties Metric English Comments
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149-97
Descriptive Properties Value Comments
Color Transparent Natural