Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® HI-1001BP PC/ABS, Metal Plating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/ABS material for platingInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 32 g/10 min

@Load 10.0 kg,
Temperature 250 °C
32 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Yield 53.9 MPa
7820 psi
50 mm/min; ASTM D638
Elongation at Break 110 %
110 %
50 mm/min; ASTM D638
Flexural Strength 78.5 MPa
11400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.59 J/cm

@Thickness 3.17 mm
10.5 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 6.40 mm
216 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 110 °C
230 °F
B/50; ISO R306