Material Notes:
Material with superior flowability and small gas generation that can be used in the exterior material of mobile phonesInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 35 g/10 min

@Load 10.0 kg,
Temperature 250 °C
35 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 52.0 MPa
7540 psi
50 mm/min; ASTM D638
Flexural Strength 73.5 MPa
10700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 4.41 J/cm

@Thickness 6.35 mm
8.27 ft-lb/in

@Thickness 0.250 in
ASTM D256
6.47 J/cm

@Thickness 3.17 mm
12.1 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 121 °C
250 °F
B/50; ISO R306