Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Water Absorption 0.20 %

@Temperature 23.0 °C
0.20 %

@Temperature 73.4 °F
ASTM D570
Melt Flow 55 g/10 min

@Load 10.0 kg,
Temperature 220 °C
55 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 59.8 MPa
8680 psi
50 mm/min; ASTM D638
Flexural Strength 88.3 MPa
12800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.35 GPa
341 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.39 J/cm

@Thickness 3.17 mm
10.1 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
V-2

@Thickness 1.20 - 3.00 mm
V-2

@Thickness 0.0472 - 0.118 in
V-1

@Thickness 1.00 mm
V-1

@Thickness 0.0394 in
V-0

@Thickness 1.20 - 3.00 mm
V-0

@Thickness 0.0472 - 0.118 in
5VB

@Thickness 1.50 - 3.00 mm
5VB

@Thickness 0.0591 - 0.118 in
Users viewing this material also viewed the following: