Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphthalamide (PPA)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 2.18 g/cc
2.18 g/cc
ASTM D792
Water Absorption 10 %

@Temperature 23.0 °C
10 %

@Temperature 73.4 °F
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.4 MPa
4270 psi
5 mm/min; ASTM D638
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Flexural Modulus 10.8 GPa
1560 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.196 J/cm

@Thickness 3.17 mm
0.367 ft-lb/in

@Thickness 0.125 in
ASTM D256