Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® XP-4240 PPS/PPA

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphthalamide (PPA)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XP-4240 PPS/PPA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 127 MPa
18500 psi
5 mm/min; ASTM D638
Flexural Strength 157 MPa
22800 psi
2.8 mm/min; ASTM D638
Flexural Modulus 11.8 GPa
1710 ksi
2.8 mm/min; ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 270 °C

@Thickness 6.40 mm
518 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 - 3.00 mm
V-0

@Thickness 0.0315 - 0.118 in
Users viewing this material also viewed the following: