Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
50 mm/min; ASTM D638
Flexural Strength 51.0 MPa
7400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.81 GPa
263 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.94 J/cm

@Thickness 3.17 mm
5.51 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 91.0 °C
196 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 3.00 mm
HB

@Thickness 0.0591 - 0.118 in