Samsung Cheil Industries Starex® HF-5661H ASA, Unreinforced  (discontinued **)

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® HF-5661H ASA, Unreinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amorphous Styrene Acrylonitrile (SAN)Characteristics: High Flow: Impact, Heat and Chemical Resistance and Surface GlossApplications: Pens, TV Components, Refrigerator and Appliance ComponentsProcessing: Injection Molding (Melt Temperature: 460-500°F, Mold Temperature: 100-175°F)Starex® is a registered trademark of Cheil Industries, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Melt Flow 1.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Tensile Strength at Break 72.6 MPa
10500 psi
ASTM D638
Elongation at Break 4.6 %
4.6 %
ASTM D638
Flexural Yield Strength 114.7 MPa
16640 psi
ASTM D790
Flexural Modulus 3.17 GPa
460 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 105 °C
221 °F
ASTM D1525
Flammability, UL94 HB
HB
0.125 in
Processing Properties Metric English Comments
Melt Temperature 238 - 260 °C
460 - 500 °F
Injection
Mold Temperature 38.0 - 79.0 °C
100 - 174 °F