Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® NA-0660I ABS, Unreinforced Anti-Bacteria Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nano-silver high flowability antibacterial ABS that can be used in notebook keyboardsInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 3.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 38.2 MPa
5550 psi
5 mm/min; ASTM D638
Elongation at Break 30 %
30 %
5 mm/min; ASTM D638
Flexural Strength 57.9 MPa
8400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.16 J/cm

@Thickness 6.35 mm
4.04 ft-lb/in

@Thickness 0.250 in
ASTM D256
3.43 J/cm

@Thickness 3.17 mm
6.43 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C

@Thickness 6.40 mm
180 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 99.0 °C
210 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in