Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 7.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 32.4 MPa
4690 psi
20 mm/min; ASTM D638
Elongation at Break 80 %
80 %
20 mm/min; ASTM D638
Flexural Strength 44.1 MPa
6400 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.57 GPa
228 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.588 J/cm

@Thickness 6.35 mm
1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
0.686 J/cm

@Thickness 3.17 mm
1.29 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 97.0 °C
207 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 3.20 mm
HB

@Thickness 0.0591 - 0.126 in
Users viewing this material also viewed the following: