Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® WR-9700S ASA, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in golf cart roof etc.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Melt Flow 8.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength, Yield 42.2 MPa
6120 psi
5 mm/min; ASTM D638
Flexural Strength 61.8 MPa
8960 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 4.22 J/cm

@Thickness 3.17 mm
7.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 98.0 °C
208 °F
B/50; ISO R306
Copyright © lookpolymers.com All Rights Reserved