Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210 is a general purpose grade.Applications:Automotive gear level housingConnectorsCable tiesHarness clipsTubesFastenersCastor wheelsHose clipsVacuum hoseHood stayInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 1.4 %
1.4 %
ASTM D570
Linear Mold Shrinkage 0.011 - 0.014 cm/cm
0.011 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 85.3 MPa
12400 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 108 MPa
15600 psi
ASTM D790
Flexural Modulus 2.70 GPa
391 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 233 °C
451 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149