Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samyang Tramid® 910 PA66/PA6

Category Polymer , Thermoplastic , Nylon
Manufacturer Samyang
Trade Name Tramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tramid® 910 PA66/PA6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.Applications:Automotive knob types, door handles and mirror housingsConnectorsCable tiesHarness clipsTubesFastenersCastor wheelsHose clipsVacuum hoseHood stayInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.4 %
1.4 %
ASTM D570
Linear Mold Shrinkage 0.015 - 0.017 cm/cm
0.015 - 0.017 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 64.7 MPa
9390 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 147 MPa
21300 psi
ASTM D790
Flexural Modulus 8.14 GPa
1180 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 261 °C
502 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 192 °C
378 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
ASTM D648