Material Notes:
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor recreation equipments. TRIEL® can be processed by a variety of thermoplastic processing techniques like injection molding, extrusion and extrusion blow molding.Grade Characteristics:High ElasticityGood SpinningUV StabilityGood DyingApplications:Elastic FiberAll information provided by Samyang
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Water Absorption 0.45 %

@Time 86400 sec
0.45 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.014 - 0.015 cm/cm
0.014 - 0.015 in/in
ASTM D955
Melt Flow 15 - 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 - 18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D2240
Tensile Strength, Yield 2.16 - 2.35 MPa

@Strain 5.00 %
313 - 341 psi

@Strain 5.00 %
ASTM D638
4.22 - 4.41 MPa

@Strain 10.0 %
612 - 640 psi

@Strain 10.0 %
ASTM D638
7.65 - 7.85 MPa

@Strain 50.0 %
1110 - 1140 psi

@Strain 50.0 %
ASTM D638
Elongation at Break >= 400 %
>= 400 %
ASTM D638
Flexural Yield Strength 3.92 MPa
569 psi
ASTM D638
Flexural Modulus 0.0226 GPa
3.27 ksi
ASTM D790
Izod Impact, Unnotched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D256
NB

@Temperature -23.0 °C
NB

@Temperature -9.40 °F
ASTM D256
Taber Abrasion, mg/1000 Cycles 32
32
CS-17 Wheel; ASTM D1044
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
Rate B; ASTM D648
Vicat Softening Point 143 °C

@Load 1.02 kg
289 °F

@Load 2.25 lb
Rate B; ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 170 - 220 °C
338 - 428 °F
Injection or Extrusion
Middle Barrel Temperature 180 - 220 °C
356 - 428 °F
Injection
190 - 230 °C
374 - 446 °F
Extrusion
Front Barrel Temperature 180 - 220 °C
356 - 428 °F
Injection
190 - 220 °C
374 - 428 °F
Extrusion
Nozzle Temperature 180 - 220 °C
356 - 428 °F
Injection
Die Temperature 190 - 220 °C
374 - 428 °F
Extrusion
Drying Temperature <= 100 °C
<= 212 °F
Dry Time 3 - 4 hour
3 - 4 hour
Moisture Content <= 0.030 %
<= 0.030 %
Injection Pressure 5.90 - 7.90 MPa
856 - 1150 psi
Cycle Time - Injection 1.2 - 1.5 sec
1.2 - 1.5 sec
Cycle Time - Cooling 10 - 20 sec
10 - 20 sec