Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sawbones Fourth-Generation Simulated Cortical Bone (Short Fiber Filled Epoxy)

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Epoxy , Epoxy, Molded, Glass Fiber Filler , Filled/Reinforced Thermoset
Manufacturer Sawbones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sawbones Fourth-Generation Simulated Cortical Bone (Short Fiber Filled Epoxy).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rigid polyurethane foam cancellous core material, unless cellular rigid polyurethane foam is specified. The mid-shaft area has an intermedullarly canal. Fourth-Generation Composite Bones Have Improved Properties Fourth-generation composite cortical bone has been developed in order to meet the demanding needs of in vitro experiments, fatigue testing and to more closely simulate natural cortical bone. The result is a composite bone with enhancements to the following properties: Fracture Toughness - Fatigue Crack Resistance Fatigue Life - Implant Subsidence Tensile Strength & Modulus - Compressive Strength & Modulus Thermal Stability - Moisture Resistance No changes have been made to the anatomical structure of the bones.Information provided by Sawbones.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 93.0 MPa
13500 psi
Transverse; ASTM D638
106 MPa
15400 psi
Longitudinal; ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
Transverse; ASTM D638
16.0 GPa
2320 ksi
Longitudinal; ASTM D638
Compressive Strength 157 MPa
22800 psi
ASTM D695
Compressive Modulus 16.7 GPa
2420 ksi
ASTM D695