Material Notes:
SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Viscosity Test 150 cm³/g
150 cm³/g
H<sub>2</sub>SO<sub>4</sub>; ISO 307
Mechanical Properties Metric English Comments
Tensile Strength 195 MPa
28300 psi
5 mm/min; ISO 527-1
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527-1
Tensile Modulus 12.2 GPa
1770 ksi
1 mm/min; ISO 527-1
Flexural Strength 307 MPa
44500 psi
2 mm/min; ISO 178
Flexural Modulus 10.0 GPa
1450 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
14.0 kJ/m²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²

@Temperature -30.0 °C
38.1 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1U
83.0 kJ/m²

@Temperature 23.0 °C
39.5 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
8.50 J/cm²

@Temperature -30.0 °C
40.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 209 °C
408 °F
80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 216 °C
421 °F
B/120; ISO 306
Processing Properties Metric English Comments
Melt Temperature 260 - 290 °C
500 - 554 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C

@Time 7200 - 21600 sec
176 °F

@Time 2.00 - 6.00 hour
Moisture Content <= 0.20 %
<= 0.20 %