Schott BG26 Band Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott BG26 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.56 g/cc
0.0925 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.80 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.89 µin/in-°F

@Temperature -22.0 - 158 °F
10.3 µm/m-°C

@Temperature 20.0 - 300 °C
5.72 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 494 °C
921 °F
Optical Properties Metric English Comments
Refractive Index 1.50

@Wavelength 1014 nm
1.50

@Wavelength 1014 nm
Hg
1.51

@Wavelength 587.6 nm
1.51

@Wavelength 587.6 nm
He
1.53

@Wavelength 404.7 nm
1.53

@Wavelength 404.7 nm
Hg
Transmission, Visible 60 %

@Wavelength 690 nm
60 %

@Wavelength 690 nm
92 %

@Wavelength 400 - 500 nm
92 %

@Wavelength 400 - 500 nm
Internal transmittance of 100% from 400-500 nm
IR Transmittance 90 %

@Wavelength 2000 - 2100 nm
90 %

@Wavelength 2000 - 2100 nm
Internal transmittance of 98% from 2000-2100 nm.
UV Transmittance <= 0.040 %

@Wavelength 200 - 280 nm
<= 0.040 %

@Wavelength 200 - 280 nm
92 %

@Wavelength 380 - 390 nm
92 %

@Wavelength 380 - 390 nm
Internal transmittance of 100%  from 380-390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0