Schott N-SF57HT Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott N-SF57HT Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.53 g/cc
0.128 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 520
520
.1/20
Modulus of Elasticity 96.0 GPa
13900 ksi
Poissons Ratio 0.26
0.26
Shear Modulus 38.0 GPa
5510 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.72 µin/in-°F

@Temperature -22.0 - 158 °F
9.90 µm/m-°C

@Temperature 20.0 - 300 °C
5.50 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.660 J/g-°C
0.158 BTU/lb-°F
Thermal Conductivity 0.990 W/m-K
6.87 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 629 °C
1160 °F
Optical Properties Metric English Comments
Refractive Index 1.84666

@Wavelength 587.6 nm
1.84666

@Wavelength 587.6 nm
n<sub>d</sub>
1.85004

@Wavelength 546.1 nm
1.85004

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 38.2 %

@Thickness 10.0 mm,
Wavelength 380 nm
38.2 %

@Thickness 0.394 in,
Wavelength 380 nm
83.1 %

@Thickness 10.0 mm,
Wavelength 405 nm
83.1 %

@Thickness 0.394 in,
Wavelength 405 nm
95.1 %

@Thickness 10.0 mm,
Wavelength 460 nm
95.1 %

@Thickness 0.394 in,
Wavelength 460 nm
99.1 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.1 %

@Thickness 0.394 in,
Wavelength 580 nm
99.2 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.2 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 86.7 %

@Thickness 10.0 mm,
Wavelength 2500 nm
86.7 %

@Thickness 0.394 in,
Wavelength 2500 nm
99.5 %

@Thickness 10.0 mm,
Wavelength 1530 nm
99.5 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 0.30 %

@Thickness 10.0 mm,
Wavelength 365 nm
0.30 %

@Thickness 0.394 in,
Wavelength 365 nm
6.3 %

@Thickness 10.0 mm,
Wavelength 370 nm
6.3 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 1.0
1.0
Alkali Class, AR 1.0
1.0
Stain Resistance Class, FR 0.00
0.00
Descriptive Properties Value Comments
B 0
Climatic Resistance Test CR 1
HG 4
K (10-6mm2/N) 2.78
Phosphate Resistance PR 1
T1013.0 (°C) 616
T107.6 (°C) 716