Schott VG6 Band Pass Filter

Category Ceramic , Glass , Optical , Filter
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott VG6 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.90 g/cc
0.105 lb/in³
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
10.6 µm/m-°C

@Temperature 20.0 - 300 °C
5.89 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 470 °C
878 °F
Optical Properties Metric English Comments
Refractive Index 1.55

@Wavelength 587.6 nm
1.55

@Wavelength 587.6 nm
He
1.56

@Wavelength 480 nm
1.56

@Wavelength 480 nm
Cd
Transmission, Visible <= 4.0 %

@Wavelength 400 nm
<= 4.0 %

@Wavelength 400 nm
76 %

@Wavelength 520 nm
76 %

@Wavelength 520 nm
Internal transmittance of 84% at 520 nm
IR Transmittance 85 %

@Wavelength 2300 - 2700 nm
85 %

@Wavelength 2300 - 2700 nm
Internal transmittance of 93% from 2300-2600 nm.
UV Transmittance <= 0.20 %

@Wavelength 200 - 320 nm
<= 0.20 %

@Wavelength 200 - 320 nm
0.40 %

@Wavelength 330 nm
0.40 %

@Wavelength 330 nm
Internal transmittance of 0.4% at 330 nm
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0