Material Notes:
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type 1 (Viton A)Chemical and heat resistantViton® is a registered trademark of DuPont. Information provided by Seals Eastern.
Physical Properties Metric English Comments
Specific Gravity 1.83 g/cc
1.83 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A >= 85
>= 85
ASTM D2240
95
95
Average; ASTM D2240
96
96
Dry Heat Aging 392°F; 70 hr; ASTM D865
Tensile Strength >= 9.908 MPa
>= 1437 psi
ASTM D412 Method A
13.05 MPa
1893 psi
Average; ASTM D412 Method A
13.97 MPa
2026 psi
Dry Heat Aging 392°F; 70 hr; ASTM D865
Tensile Stress 5.10 MPa

@Strain 25.0 %
740 psi

@Strain 25.0 %
Average; ASTM D412 Method A
>= 5.86 MPa

@Strain 50.0 %
>= 850 psi

@Strain 50.0 %
ASTM D412 Method A
7.619 MPa

@Strain 50.0 %
1105 psi

@Strain 50.0 %
Average; ASTM D412 Method A
>= 8.27 MPa

@Strain 100 %
>= 1200 psi

@Strain 100 %
ASTM D412 Method A
10.7 MPa

@Strain 100 %
1550 psi

@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 63 %
>= 63 %
ASTM D412 Method A
97 %
97 %
Dry Heat Aging 392°F; 70 hr; ASTM D865
101 %
101 %
Average; ASTM D412 Method A
Compression Set 18 %

@Temperature 200 °C,
Time 79200 sec
18 %

@Temperature 392 °F,
Time 22.0 hour
ASTM D395, Test B
32 %

@Temperature 200 °C,
Time 252000 sec
32 %

@Temperature 392 °F,
Time 70.0 hour
ASTM D395, Test B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -27.2 °C
-17.0 °F
Retraction Temperature, TR10; ASTM D1329
Brittleness Temperature -34.4 °C
-30.0 °F
ASTM D746
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
ASTM D1329
Processing Properties Metric English Comments
Shelf Life 120 Month
120 Month
Descriptive Properties Value Comments
Strain Energy/ Unit Volume at 20% Elongation (psi) 87
ASTM D412 Method A