Seals Eastern Perflas® 9295 Perfluorinated Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Seals Eastern, Inc
Trade Name Perflas®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern Perflas® 9295 Perfluorinated Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Perfluoro rubber for high-temperature, aggressive chemical service. Perflas 9295® seals offer high temperature service and are resistant to aggressive chemicals. They are a thermally stable, perfluorinated elastomer (FFKM). Perflas 9295 seals offer outstanding resistance to high temperature (320°C/608°F). Perflas 9295 seals resist attack by nearly all chemical reagents, including organic and inorganic acids, alkalines, ketones, esters, alcohols, fuels and hot water. Information provided by Seals Eastern, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.13 g/cc
2.13 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Tensile Strength at Break 19.50 MPa
2828 psi
AVG; ASTM D412 Method A
19.89 MPa

@Temperature 200 °C,
Time 252000 sec
2885 psi

@Temperature 392 °F,
Time 70.0 hour
ASTM D865
Elongation at Break 268 %
268 %
AVG; ASTM D412 Method A
200.9 %

@Temperature 200 °C,
Time 252000 sec
200.9 %

@Temperature 392 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
100% Modulus 0.007701 GPa
1.117 ksi
Compression Set 25 %

@Temperature 23.0 °C,
Time 252000 sec
25 %

@Temperature 73.4 °F,
Time 70.0 hour
O-ring (-214) ASTM Method B
37 %

@Temperature 200 °C,
Time 252000 sec
37 %

@Temperature 392 °F,
Time 70.0 hour
O-ring (-214) ASTM Method B
45 %

@Temperature 230 °C,
Time 252000 sec
45 %

@Temperature 446 °F,
Time 70.0 hour
O-ring (-214) ASTM Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
ASTM D1329