Sekisui PIOCELAN LSP-50EB Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN LSP-50EB Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Packing material/Returnable containers for electronic parts and Automotive partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0200 g/cc
0.000723 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.3567 MPa
51.73 psi
ASTM D3575
Elongation at Break 13.4 %
13.4 %
ASTM D3575
Flexural Strength 0.1929 MPa
27.98 psi
ASTM D790
Flexural Modulus 0.0086860 GPa
1.2598 ksi
ASTM D790
Compressive Strength 0.1210 MPa

@Strain 25.0 %
17.55 psi

@Strain 25.0 %
ASTM D3575
0.1800 MPa

@Strain 50.0 %
26.11 psi

@Strain 50.0 %
ASTM D3575
0.3950 MPa

@Strain 75.0 %
57.29 psi

@Strain 75.0 %
ASTM D3575
Compression Set 32.2 %
32.2 %
ASTM D3575
Descriptive Properties Value Comments
Color Black
Range of center value of pre-expanded particles 0.13-0.19 in