Sekisui PIOCELAN OP-20DB Moldable Polymer Foam

Category Polymer , Thermoplastic , Polyolefin , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Sekisui Plastics
Trade Name PIOCELAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sekisui PIOCELAN OP-20DB Moldable Polymer Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics.Major use of Molded articles: Automotive partsInformation provided by Sekisui Plastic Co. Ltd.
Physical Properties Metric English Comments
Bulk Density 0.0500 g/cc
0.00181 lb/in³
After expansion; ASTM D3575
Mechanical Properties Metric English Comments
Tensile Strength 0.6181 MPa
89.65 psi
ASTM D3575
Elongation at Break 10.5 %
10.5 %
ASTM D3575
Flexural Strength 0.4134 MPa
59.96 psi
ASTM D790
Flexural Modulus 0.01767 GPa
2.563 ksi
ASTM D790
Compressive Strength 0.3025 MPa

@Strain 25.0 %
43.88 psi

@Strain 25.0 %
ASTM D3575
0.3872 MPa

@Strain 50.0 %
56.16 psi

@Strain 50.0 %
ASTM D3575
0.7364 MPa

@Strain 75.0 %
106.8 psi

@Strain 75.0 %
ASTM D3575
Compression Set 41.8 %
41.8 %
ASTM D3575
Descriptive Properties Value Comments
Color Black
Range of center value of pre-expanded particles 0.13-0.18 in